Power of Light
Moissanite (4H-SiC), Natural Diamond, Lab-Grown Diamond, and Cubic Zirconia benchmarked side by side.
Moissanite (4H-SiC), Natural Diamond, Lab-Grown Diamond, and Cubic Zirconia benchmarked side by side.
Move the Diamond Equivalent Weight slider below to inspect typical loose certified Color D / VVS1 stone market prices across carat brackets.
The benchmark above reflects calibrated, optically selected Color D 4H-SiC moissanite. Bargain marketplace dropshippers often attach “Color D / VVS1” titles and identical pre-printed GRA slips to cloudy rough or off-color G–J rejects. The same caution applies to discount retail stores offering sterling silver moissanite rings under $50 (or below 200 PLN in Central Europe)—these are routinely mass-produced Asian imports set with weak stones that fall noticeably short of genuine Color D brilliance.
| Property | Moissanite (4H-SiC) | Natural Diamond (C) | Lab Diamond (C) | Cubic Zirconia (ZrO₂) |
|---|---|---|---|---|
| Refractive Index (RI) | 2.65 – 2.69 (Highest) | 2.42 | 2.42 | 2.15 |
| Spectral Dispersion (Fire) | 0.104 (2.4x diamond fire) | 0.044 | 0.044 | 0.060 |
| Mohs Scratch Hardness | 9.25 / 10 (Second hardest) | 10.0 / 10 | 10.0 / 10 | 8.0 – 8.5 / 10 |
| Optical Birefringence | Anisotropic (+0.043 double refraction) | Isotropic (Single) | Isotropic (Single) | Isotropic (Single) |
| Specific Gravity | 3.22 g/cm³ (~10% lighter than diamond) | 3.52 g/cm³ | 3.52 g/cm³ | 5.6 – 6.0 g/cm³ |
| Torch Repair Resistance | Yes (reversible thermochromism above 700 °C) | Requires borax flux > 800 °C | Requires borax flux > 800 °C | Risks cracking / coating failure |
| Thermal Tester Reading | Reads as Diamond (Thermal) | Diamond | Diamond | Simulant |
| 10-Year Clouding Risk | Zero — permanent crystal lattice | Zero | Zero | High — microporous abrasion |
| Conflict-Free Ethical Traceability | 100% laboratory grown | Mixed / requires Kimberly provenance | 100% laboratory grown | 100% synthetic |
Because solid silicon carbide transfers thermal energy nearly as quickly as crystalline carbon, pocket heat-probe testers beep “Diamond” on genuine moissanite.
Only dual thermal-and-electrical conductivity testers measure wide-bandgap semiconductor conductivity alongside heat flow, cleanly separating 4H-SiC from carbon diamonds. Visually, examining kite facets through the table with a 10x loupe also reveals crisp double refraction.
Explore fine gold and platinum-plated 925 sterling silver rings at Biżuteria Pola—set strictly with optically verified Grade D / VVS1 crystals backed by individual GRA documentation.